LY-04PM ((High-Fill Series)
● The LY-04PM product is a high-performance, performance-upgraded version of the LY-18SPA product. While its finished-particle-size control is slightly lower, it features larger primary crystal grains, more complete crystal morphology, higher crystallinity, and better dispersibility. ● Compared with the LY-18SPA product, the LY-04PM product features a higher bulk density and superior self-flowability, making it more suitable for customers using automated feeding systems without clogging. ● The LY-04PM product exhibits a lower oil absorption value and higher crystallinity compared with the LY-18SPA product, resulting in superior thermal stability, water resistance, and enhanced performance in high-fill, high-flame-retardant applications. ● The LY-04PM product exhibits a higher melt index than the LY-18SPA product, resulting in superior processing performance in customer applications, lower production costs, and enhanced application performance.
Category:
Keywords:
Physical filtration, ion exchange, membrane filtration, storage systems, auxiliary systems
Product Description
Product grade |
Particle size index (µm) |
Ingredient Content (%) |
Whiteness |
Loose packing density g/cm³ |
Oil absorption value ml/100g |
Electrical conductivity us/cm |
pH value |
Residue on a 500-mesh sieve % |
||||||||
D10 |
D50 |
D90 |
D97 |
D100 |
Silicon dioxide |
Fe₂O₃ |
Sodium oxide |
Loss on ignition |
Alkaline additive |
|||||||
Indicator Requirements |
- |
1.7~2.0 |
- |
≤7.0 |
- |
≤0.02 |
≤0.02 |
≤0.20 |
34~35 |
≤0.010 |
≥97 |
≥0.38 |
≤30 |
≤100 |
≤9.5 |
≤0.003 |
LY-04PM |
0.934 |
1.794 |
3.364 |
4.263 |
8.256 |
0.004 |
0.005 |
0.090 |
34.40 |
0.0039 |
99.08 |
0.52 |
28.0 |
54.7 |
8.46 |
0.00039 |
▲ Particle size distribution of LY-04PM product; ▲ SEM image of LY-04PM product
Application specifications for low-smoke, halogen-free cable compounds:
Product grade |
Tensile strength |
Elongation at break |
Melt Index (6 g/160°C/21.6 kg) |
Volume resistivity at 20°C |
Oxygen Index |
megapascal |
% |
g/10min |
*10¹¹ Ω·m |
% |
|
LY-04PM |
13.07 |
231.65 |
11.55 |
30.03 |
33.4 |
Note: Application tests were conducted using a base formulation in which aluminum hydroxide was added at 60.6%. The base formulation is shown in the figure below.
| Materials | Mass percentage (%) | Number of copies |
| EVA | 22.7 | 45 |
| LLDPE | 9.5 | 18.75 |
| Aluminum hydroxide | 60.6 | 120 |
| Grafting material | 5.7 | 11.25 |
| Silicone masterbatch | 0.8 | 1.5 |
| 1010 | 0.4 | 0.75 |
| DLTP | 0.4 | 0.75 |
| Total | 100 | 198 |
Product Features:
● The LY-04PM product is a high-performance, performance-upgraded version of the LY-18SPA product. While its finished-particle-size control is slightly lower, it features larger primary crystal grains, more complete crystal morphology, higher crystallinity, and better dispersibility.
● Compared with the LY-18SPA product, the LY-04PM product features a higher tapped density and superior self-flow characteristics, making it more suitable for customers using automated feeding systems without clogging.
● The LY-04PM product exhibits a lower oil absorption value and higher crystallinity compared with the LY-18SPA product, resulting in superior thermal stability, enhanced resistance to water erosion, and excellent high-fill, high-flame-retardant performance in application.
● The LY-04PM product exhibits a higher melt index than the LY-18SPA product, resulting in superior processing performance in customer applications, lower production costs, and enhanced application performance.